This leaky roof was fixed in 20 minutes with Polaroof RAC and Roofab.  First, a coat of Polaroof RAC was applied to the flashing detail. by brush and roller.

Andek Polaroof RAC

ROOFAB was laid into the wet coating, positioned and then topcoated with POLAROOF RAC.

Andek Polaroof RAC

A larger piece of ROOFAB was cut to patch a cracked and worn area. The same application procedure described above (POLAROOF RAC, ROOFAB, POLAROOF RAC) was followed.

Andek Polaroof RAC

The roof was then thoroughly coated with POLAROOF RAC at approximately 100 sq. ft. per gallon, as a basecoat. The roof was recoated the next day at the same rate to provide the appropriate 24/25 dry mils thickness.

Andek Polaroof RAC

Here is the finished roof. Notice the larger piece of ROOFAB in the foreground that was used to patch the cracked and worn area of the roof. With this application procedure completed, you now have installed a 10 year roof surface that is FM approved, Class "A" fire rated and seamless.

The original roof had weathered badly from UV exposure.  Silver coating had worn off and bugholes from UV deterioration and bird pecking were evident everywhere.

Andek Polaroof RAC
Using DRY sand, you can mix up a dry, crumbly grout with POLAROOF RAC to patch holes and fill cracks as part of the preparation before applying two coats of POLAROOF RAC. Andek Polaroof RAC
Flashing details around pipes, air conditioners and roof penetrations must be performed as part of the preparation.  These areas should be reinforced with ROOFAB. Andek Polaroof RAC

Finally, the roof is coated with two coats of POLAROOF RAC  to provide a 10 year roof restoration.

Andek Polaroof RAC
Andek Polaroof RAC Andek Polaroof RAC
Andek Polaroof RAC Andek Polaroof RAC

ABOVE: S.H. Contractors, Ceramic Mfg Facility, Woodbridge, NJ. Polaprime 2, Polaroof RAC and Roofab applied over PUF, modified capsheet, transite and metal surfaces (approx 100,000 sq ft).

Andek Polaroof RAC Andek Polaroof RAC